Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | >= 0.00400 GPa | >= 0.580 ksi | DIN 53504 |
NEXA® PFX8012 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | >= 0.00400 GPa | >= 0.580 ksi | DIN 53504 |
NEXA® PFX9014 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
Termopol Termoton® V5GA1090A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 527 |
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane Pearlbond™ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials Pearlthane® D91T80 Thermoplastic Polyurethane Type : Pearlthane® D91T80 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties... |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
Mearthane Durethaneâ„¢ S DS-285A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 527 |
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane Pearlbond™ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low soft.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-A880 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00400 GPa @Temperature 100 °C |
0.580 ksi @Temperature 212 °F |
10 weeks, Heat Resistance |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
Lubrizol ESTANE® GP75AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 75AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
ELASTO UK Dryflex® 400801S SBS Based Material, 80A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
ELASTO UK Dryflex® 402801S SBS Based Material, 80A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
ELASTO UK Dryflex® 500800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
ELASTO UK Dryflex® 502800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
ELASTO UK Dryflex® 600800S SEBS Based Material, Filled Qualities, 80A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
ELASTO UK Dryflex® 602800S SEBS Based Material, Filled Qualities, 80A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D638 |
ELASTO UK Dryflex® 660800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 ASTM D3568 FormulationNordel® IP 5565 |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 5565 Heat Resistant Peroxide Cured FormulationNordel® IP 5565 |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | Vulcanizate, Press cured, TC95 +3min at 180°C |
Dow Nordel® IP 4570 Heat Resistant Peroxide Compound FormulationNordel® IP 4570 |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D 638 |
API Megol AM DP2217/90PBT SEBS Adhesion Modified Overmolding for Polyesters Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ISO 37 |
AlphaGary Evoprene™ Super G 932 SEBS Thermoplastic Elastomer Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1580 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
100% Modulus | 0.00400 GPa | 0.580 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-2180 Polycaprolactone Based TPU Low compression set, good oil resistance & hydrolytic stability, good abrasion resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |