Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlbond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlbondâ„¢ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrusion and compounding. Applications: Pearlbondâ„¢ 12F75UV is designed for a wide variety of adhesive film applications requiring excellent adhesion in combination with good heat resistance and dry cleaning resistance. This grade can be both cast extruded and blown.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ISO 2781
Melt Flow 40 - 60 g/10 min

@Load 10.0 kg,
Temperature 190 °C
40 - 60 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
ISO 527
Elongation at Break 525 %
525 %
ISO 527
100% Modulus 0.00400 GPa
0.580 ksi
ISO 527
300% Modulus 0.00700 GPa
1.02 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 130 - 140 °C
266 - 284 °F
MQSA 70 A
Softening Point 110 - 130 °C
230 - 266 °F
MQSA 70 A
Processing Properties Metric English Comments
Zone 1 145 - 155 °C
293 - 311 °F
Zone 2 155 - 165 °C
311 - 329 °F
Zone 3 165 - 170 °C
329 - 338 °F
Zone 4 170 - 180 °C
338 - 356 °F
Die Temperature 170 - 180 °C
338 - 356 °F