Mechanical Properties Metric English Comments
100% Modulus 0.00410 GPa
0.595 ksi
DIN 53504
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec..
100% Modulus 0.00410 GPa
0.595 ksi
Freudenberg Simrit Superiorâ„¢ F815 Fluoroelastomer
Cost-effective, high performance compound for semiconductor applications. It offers outstanding plasma resistance and low particulation in a wide range of plasma environments.
100% Modulus 0.00410 GPa

@Temperature 23.0 °C
0.595 ksi

@Temperature 73.4 °F
12 months, Weathering @ 45° South, 25 mil - Natural, Arizona
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..
100% Modulus 0.00410 GPa
0.595 ksi
ASTM D412/D638
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and..
100% Modulus 0.00410 GPa
0.595 ksi
ASTM D412
Elastocon TPE Technologies Elastocon® 8068L Thermoplastic Elastomer
Elastocon® 8068L is a colorable lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068L is well ..
100% Modulus 0.00410 GPa
0.595 ksi
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
DuPont Performance Polymers VTR 8650 (GBL-S) Peroxide Cured Fluoroelastomer (FKM) Formulation
FormulationVTR 8650
100% Modulus 0.00410 GPa
0.595 ksi
ASTM D412
Advanced Polymer Alloys Alcryn® 2180 BK Melt Processable Rubber