Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00410 GPa | 0.595 ksi | DIN 53504 |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
100% Modulus | 0.00410 GPa | 0.595 ksi | |
Freudenberg Simrit Superiorâ„¢ F815 Fluoroelastomer Cost-effective, high performance compound for semiconductor applications. It offers outstanding plasma resistance and low particulation in a wide range of plasma environments. |
|||
100% Modulus | 0.00410 GPa @Temperature 23.0 °C |
0.595 ksi @Temperature 73.4 °F |
12 months, Weathering @ 45° South, 25 mil - Natural, Arizona |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
100% Modulus | 0.00410 GPa | 0.595 ksi | ASTM D412/D638 |
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and.. |
|||
100% Modulus | 0.00410 GPa | 0.595 ksi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8068L Thermoplastic Elastomer Elastocon® 8068L is a colorable lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068L is well .. |
|||
100% Modulus | 0.00410 GPa | 0.595 ksi | Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8650 (GBL-S) Peroxide Cured Fluoroelastomer (FKM) Formulation FormulationVTR 8650 |
|||
100% Modulus | 0.00410 GPa | 0.595 ksi | ASTM D412 |
Advanced Polymer Alloys Alcryn® 2180 BK Melt Processable Rubber Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades.. |