Shin-Etsu Silicones SFX-14036AU Fluorosilicone Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Shin-Etsu Silicones
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shin-Etsu Silicones SFX-14036AU Fluorosilicone Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description Shincor SFX14036AU is normal 75 Durometer fluorosilicone compounds. It is designed to process well in molding applications. Product Features: Excellent fuel and solvent resistance.Usable over a broad temperature range.Information Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.63 g/cc
1.63 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Tensile Strength at Break 7.24 MPa
1050 psi
100% Modulus 0.00586 GPa
0.850 ksi
Descriptive Properties Value Comments
Cure Agent DBPH
Cure Type Post Cure
Copyright © lookpolymers.com All Rights Reserved