Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 0.00680 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00680 GPa
0.986 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00680 GPa
0.986 ksi
ASTM D412
Mearthane Durethaneâ„¢ S DS-390A Solid Polyurethane Elastomer
TDI backbone: ether.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
100% Modulus 0.00680 GPa
0.986 ksi
Press-cured 5 minutes at 190°C
DuPont Vamac® DP HVA-2 Coagent Test Compound
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper..
100% Modulus 0.00680 GPa
0.986 ksi
Air aged 7 days at 150°C
DuPont Vamac® GLS Sample Compound Vulcanizate Slab Cured
Test slab is press cured for 5 minutes at 177°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for thei..
100% Modulus 0.00680 GPa
0.986 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00680 GPa
0.986 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR8520 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
100% Modulus 0.00680 GPa
0.986 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR9060EF PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..