Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D412 |
S&E Specialty Polymers GA-1042LF PVC Application: UL bulletinized PVC based compound, suitable for injection molding application.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D412 |
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | DIN 53504 |
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | DIN 53504 |
Lubrizol ESTANE® 5715F2 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D638 |
Colorite Polymers 8534 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D638 |
Colorite Polymers 9588 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D-638 |
Axiall 13870 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20.. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D-638 |
Axiall 13872 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75°C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in .. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D-638 |
Axiall 13880 Wire & Cable Flexible PVC Insulation compound suitable for 75C, oil I applications. UL recognized component for TW, Oil I and 720 hour sunlight resistant applications.Information provided by Georgia GulfGeorgia Gulf became .. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D-638 |
Axiall 14910 Wire & Cable Flexible PVC Flame retardant jacket compound recommended for CM, CL2 type constructions when used over FR-PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D-638 |
Axiall 19910 Wire & Cable Flexible PVC THHN-THWN, best suited for larger sizes (16 AWG and larger).Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D412 |
3M 5010 Polyurethane Multi-Purpose Adhesive 3M™ Polyurethane Multi-Purpose Adhesive 5010 is a one component, fast curing adhesive which forms a rigid permanent bond. 3M 5010 bonds to a wide variety of materials including wood, foam panels, f.. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D-638 |
Axiall 12870 Wire & Cable Flexible PVC 70°C oil, 80°C dry rated liquid tight conduit jacket meeting the requirements of UL 360.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D-638 |
Axiall 1055 Wire & Cable Flexible PVC NM-B and UF-B jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D-638 |
Axiall 19935 Wire & Cable Flexible PVC THHN-THWN, larger sizes. Microbe resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ASTM D-638 |
Axiall 34311 Coax & Telecom Flexible PVC CMR riser jacket over PVC or flame retardant PE insulation. Recommended for 75C applications. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorg.. |
|||
100% Modulus | 0.0117 GPa | 1.70 ksi | ISO 37 |
Lubrizol ESTANE® 58141 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |