Material Notes:
NM-B and UF-B jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 84 - 90
84 - 90
delayed; ASTM D-2240
Tensile Strength, Yield 19.3 MPa
2800 psi
ASTM D-638
Elongation at Yield 252 %
252 %
Air Aging: 10 days @ 100°C; 75-mil plaques; UL 1581
300 %
300 %
ASTM D-638
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -32.0 °C
-25.6 °F
ASTM D-746
Oxygen Index 24 %
24 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 185 °C
365 °F