Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1 hour | 5740 MPa | 833000 psi | |
Arkema Group Orgalloy® RS 6030 AT Nylon 6 Alloy, 30% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties... |
|||
Tensile Creep Modulus, 1 hour | 5740 MPa | 833000 psi | ISO 899-1 |
Arkema Group Orgalloy® RS 6030 Polyamide 6 Alloy 30% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Tensile Creep Modulus, 1 hour | 5740 MPa | 833000 psi | |
Arkema Group Orgalloy® RS 6030 Nylon 6 Alloy, 30% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |