Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.0110 - 2.07 GPa | 1.60 - 300 ksi | Average value: 0.243 GPa Grade Count:12 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Modulus of Elasticity | 0.0110 - 0.700 GPa | 1.60 - 102 ksi | Average value: 0.0939 GPa Grade Count:21 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Modulus of Elasticity | 0.0110 GPa | 1.60 ksi | ASTM D412 Method A |
Seals Eastern 7265D Fluorocarbon-Elastomer Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc. |
|||
Modulus of Elasticity | 0.0110 GPa | 1.60 ksi | Molded sample |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Modulus of Elasticity | 0.0110 GPa | 1.60 ksi | |
AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Modulus of Elasticity | 0.0110 GPa | 1.60 ksi | |
AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Modulus of Elasticity | 0.0110 - 0.413 GPa | 1.60 - 59.9 ksi | Average value: 0.179 GPa Grade Count:28 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |
|||
Modulus of Elasticity | 0.0110 GPa | 1.60 ksi | |
DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |