Modulus of Elasticity 2.40 - 8.50 GPa
348 - 1230 ksi
Average value: 4.67 GPa Grade Count:29
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Modulus of Elasticity 2.10 - 8.50 GPa
305 - 1230 ksi
Average value: 4.73 GPa Grade Count:8
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 4.50 - 8.50 GPa
653 - 1230 ksi
Average value: 6.81 GPa Grade Count:19
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..