Mechanical Properties Metric English Comments
Modulus of Elasticity 1.90 - 9.31 GPa
276 - 1350 ksi
Average value: 5.50 GPa Grade Count:21
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Modulus of Elasticity 1.93 - 9.31 GPa
280 - 1350 ksi
Average value: 2.54 GPa Grade Count:42
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Modulus of Elasticity 0.800 - 9.31 GPa
116 - 1350 ksi
Average value: 2.08 GPa Grade Count:120
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..