Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 12.0 - 14.0 GPa
1740 - 2030 ksi
Compression; ISO 527
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Modulus of Elasticity 10.0 - 14.0 GPa
1450 - 2030 ksi
Injection; ISO 527
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Modulus of Elasticity 10.0 - 14.0 GPa
1450 - 2030 ksi
Injection; ISO 527
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Modulus of Elasticity 2.60 - 14.0 GPa
377 - 2030 ksi
Average value: 6.52 GPa Grade Count:156
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Modulus of Elasticity 0.00159 - 14.0 GPa
0.230 - 2030 ksi
Average value: 2.19 GPa Grade Count:16
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Modulus of Elasticity 5.40 - 14.0 GPa

@Temperature 60.0 - 150 °C
783 - 2030 ksi

@Temperature 140 - 302 °F
Average value: 9.23 GPa Grade Count:1
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Modulus of Elasticity 3.20 - 14.0 GPa
464 - 2030 ksi
Average value: 5.74 GPa Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..