Mechanical Properties Metric English Comments
Modulus of Elasticity 3.20 - 3.50 GPa
464 - 508 ksi
ASTM D638-04
Proto3000 Objet RGD525 High Temperature Prototyping Polymer
Information provided by Proto3000 for their protoyping engineering services.
Modulus of Elasticity 2.25 - 3.50 GPa
327 - 508 ksi
Average value: 3.02 GPa Grade Count:53
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 0.900 - 3.50 GPa
131 - 508 ksi
Average value: 1.83 GPa Grade Count:35
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Modulus of Elasticity 0.400 - 3.50 GPa

@Temperature 40.0 - 150 °C
58.0 - 508 ksi

@Temperature 104 - 302 °F
Average value: 1.37 GPa Grade Count:5
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Modulus of Elasticity 3.00 - 3.50 GPa
435 - 508 ksi
Hybrid Plastics POSS® EP 1000 Epoxy Adhesive
EP1000 is a POSS® based epoxy adhesive with outstanding oxidative resistance to ozone, plasma, or atomic oxygen environments. The EP1000 POSS® Epoxy is also well-suited for peroxide and steam...
Modulus of Elasticity 3.00 - 3.50 GPa
435 - 508 ksi
Hybrid Plastics POSS® EP 1050 Epoxy Adhesive
EP1050 is a POSS® based, high-temperature epoxy adhesive with outstanding resistance to ozone, plasma, or atomic oxygen environments. Major applications include medical devices, optics, semicondu..
Modulus of Elasticity 0.350 - 3.50 GPa
50.8 - 508 ksi
Average value: 1.45 GPa Grade Count:44
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Modulus of Elasticity 1.30 - 3.50 GPa
189 - 508 ksi
Average value: 2.72 GPa Grade Count:5
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..
Modulus of Elasticity 0.750 - 3.50 GPa
109 - 508 ksi
Average value: 1.35 GPa Grade Count:43
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
Copyright © lookpolymers.com All Rights Reserved