Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hybrid Plastics POSS® EP 1000 Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Hybrid Plastics
Trade Name POSS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hybrid Plastics POSS® EP 1000 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EP1000 is a POSS® based epoxy adhesive with outstanding oxidative resistance to ozone, plasma, or atomic oxygen environments. The EP1000 POSS® Epoxy is also well-suited for peroxide and steam. It provides an exceptional transparent adhesive in these conditions for metallic, molded plastic and composite materials.Information provided by Hybrid Plastics
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
after cure
Viscosity <= 5000 cP
<= 5000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 80 - 85
80 - 85
Modulus of Elasticity 3.00 - 3.50 GPa
435 - 508 ksi
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 20.0 °C
27.8 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg 100 - 110 °C
212 - 230 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 6.00 min

@Temperature 80.0 °C
0.100 hour

@Temperature 176 °F
Pot Life 180 min
180 min
Shelf Life 6.00 - 12.0 Month
6.00 - 12.0 Month
Users viewing this material also viewed the following: