Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.14 - 15.4 GPa | 600 - 2230 ksi | Average value: 7.89 GPa Grade Count:34 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Modulus of Elasticity | 4.14 - 24.1 GPa | 600 - 3500 ksi | Average value: 10.1 GPa Grade Count:55 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Modulus of Elasticity | 4.14 - 8.96 GPa | 600 - 1300 ksi | Average value: 6.96 GPa Grade Count:13 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Modulus of Elasticity | 4.14 GPa | 600 ksi | |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
Modulus of Elasticity | 4.14 GPa | 600 ksi | |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |
|||
Modulus of Elasticity | 4.14 GPa | 600 ksi | |
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati.. |
|||
Modulus of Elasticity | 4.14 - 8.27 GPa | 600 - 1200 ksi | Average value: 6.18 GPa Grade Count:6 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |