Mechanical Properties Metric English Comments
Modulus of Elasticity 2.41 GPa
350 ksi
ASTM D638
Novatec Novaloy® 9000 PVC + ABS
Novaloy® 9000 is a specialty engineering alloy of ABS/PVC designed for injection molding, profile and sheet extrusion. Novaloy® 9000 has been formulated to provide excellent processing characte..
Modulus of Elasticity 2.41 - 2.81 GPa

@Temperature 30.0 - 120 °C
350 - 408 ksi

@Temperature 86.0 - 248 °F
Average value: 1.78 GPa Grade Count:1
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 2.41 - 2.81 GPa

@Thickness 1.50 - 4.00 mm
350 - 408 ksi

@Thickness 0.0591 - 0.157 in
Average value: 1.78 GPa Grade Count:1
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Modulus of Elasticity 2.41 - 3.65 GPa
350 - 530 ksi
Average value: 3.17 GPa Grade Count:8
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Modulus of Elasticity 2.41 - 4.50 GPa
350 - 653 ksi
Average value: 3.73 GPa Grade Count:7
Overview of materials for Thermoplastic Polyimide, Unfilled
Modulus of Elasticity 2.41 - 4.14 GPa
350 - 600 ksi
Average value: 3.58 GPa Grade Count:17
Overview of materials for Nylon 66, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri..
Modulus of Elasticity 2.41 - 11.0 GPa
350 - 1600 ksi
Average value: 4.79 GPa Grade Count:42
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Modulus of Elasticity 2.41 GPa
350 ksi
Hybrid Plastics Nanoreinforced® POSS® 5% POSS-polyimide
Nanoreinforced® POSS® Polyimide is a hybrid nanocomposite that can serve as oxidation resistant and highly bondable form of polyimide. Upon exposure to oxidizing oxygen the POSS® polyimide ..
Modulus of Elasticity 2.41 GPa
350 ksi
Secant; ASTM D882
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating
Parylene N, poly(para-xylylene), is a completely linear, highly crystalline material. Parylene N is a primary dielectric, exhibiting a very low dissipation factor, high dielectric strength, and a lo..
Modulus of Elasticity 2.41 - 13.8 GPa
350 - 2000 ksi
Average value: 6.03 GPa Grade Count:86
Overview of materials for Polycarbonate, Glass + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value..
Modulus of Elasticity 2.41 GPa
350 ksi
ASTM D790
Chesterton ARC CS2 Low-viscosity, Composite concrete primer sealer