Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.500 - 4.90 GPa @Temperature 60.0 - 90.0 °C |
72.5 - 711 ksi @Temperature 140 - 194 °F |
Average value: 1.37 GPa Grade Count:5 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |