Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 9.80 GPa | 1420 ksi | |
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Modulus of Elasticity | 9.80 GPa | 1420 ksi | ISO 527-2 |
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Modulus of Elasticity | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
BASF Ultramid® A3X4G7 35% Glass Filled PA66 FR (Dry) Description: 35% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stiffness and stre.. |
|||
Modulus of Elasticity | 9.80 GPa | 1420 ksi | ISO 527-1/-2 |
BASF Ultramid® A3X4G7 BK 23079 35% Glass Filled PA66 FR (Dry) Description: 35% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stiffness and stre.. |
|||
Modulus of Elasticity | 9.80 GPa | 1420 ksi | ISO 527-2 |
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab.. |