Mechanical Properties Metric English Comments
Charpy Impact 40.7 J

@Temperature -40.0 °C
30.0 ft-lb

@Temperature -40.0 °F
Universal Wire Works E81T1-Ni2 Flux Cored Carbon Steel Tubular Electrode
Alloys 81T1-Ni1 and Ni2 are designed for gas-shielded flux cored welding of low alloy steels that require good CVN toughness at subzero temperatures. These alloys are excellent for single and multip..
Charpy Impact 40.7 J
30.0 ft-lb
Wingate Alloys Winco-Tuf 40IT Ultra High Strength, Thru-Hardened Alloy Wear Plate
For extreme abrasion and moderate impact.Winco-Tuf 40 has excellent toughness at high hardness and in heavy sections. For severe impact and abrasions.Advantages: Maximum resistance to abrasion and i..
Charpy Impact 40.7 J

@Temperature -28.9 °C
30.0 ft-lb

@Temperature -20.0 °F
Universal Wire Works E81T1-Ni1 Flux Cored Carbon Steel Tubular Electrode
Alloys 81T1-Ni1 and Ni2 are designed for gas-shielded flux cored welding of low alloy steels that require good CVN toughness at subzero temperatures. These alloys are excellent for single and multip..
Charpy Impact 40.7 J

@Treatment Temp. 1070 °C
30.0 ft-lb

@Treatment Temp. 1950 °F
austenitizied at 1950°F; C-notch
Crucible Steel CRU-WEAR® Tool Steel
CRU-WEAR is an air-hardening tool steel, heat treatable to HRC 60-65. Designed as an upgrade to D2, it offers better wear resistance, greater toughness and higher attainable hardness. Compared to th..
Charpy Impact 40.7 J
30.0 ft-lb
notched
Carpenter AerMet® 100 Aged at 875°F
An alloy providing high hardness and strength combined with exceptional ductility and toughness. This alloy should be considered for aircraft and aerospace structural components requiring high stren..