Material Notes:
EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with superior performance in industrial applications. EP RAP displays extremely fast cure times with excellent adhesion to different substrates. EP RAP can be spray applied at temperatures ranging from 20ºF to 150ºF. EP RAP has excellent chemical resistance and excellent water insensitivity. EP RAP conforms to USDA and FDA guidelines for incidental food contact. Applications: EP RAP adheres well to several substrates including concrete, steel, and wood. Some typical uses include: SECONDARY CONTAINMENT WASTEWATER LAGOON AND POOL LININGS TABLE EDGING COLD STORAGE AREAS WASH BAY AND SHOWER LININGS COOLING TOWERS PETROCHEMICAL REFINERIES OILFIELD PIPELINE COATINGS WATER PROOFING SEWER LINERS MANHOLE RESTORATION INDUSTRIAL FLOORINGS ROOF COATINGS BRIDGE COATINGSPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Viscosity 450 cP
450 cP
A Side
600 cP
600 cP
B Side
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa
3310 psi
ASTM D412
Elongation at Break 375 %
375 %
ASTM D412
Adhesive Bond Strength >= 1.72 MPa
>= 250 psi
Wood (no primer), Delamination; ASTM D4541 Elcometer
2.07 MPa
300 psi
Concrete (epoxy), Concrete Failure; ASTM D4541 Elcometer
2.76 MPa
400 psi
Concrete (no primer), Concrete Failure; ASTM D4541 Elcometer
>= 6.21 MPa
>= 900 psi
Steel (epoxy primer), Primer Failure; ASTM D4541 Elcometer
>= 10.3 MPa
>= 1500 psi
Steel (no primer), Substrate Failure; ASTM D4541 Elcometer
Tear Strength 78.9 kN/m
450 pli
ASTM D412
Taber Abrasion, mg/1000 Cycles 76
76
CS17 WHEEL, 1kg per 1000 cycles; ASTM D4060
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
ASTM Pensky-Martin
Processing Properties Metric English Comments
Cure Time 0.417 - 2.50 min
0.00694 - 0.0417 hour
Tack Free Time
Gel Time 0.250 min
0.250 min
Fast
2.00 min
2.00 min
Slow
Descriptive Properties Value Comments
Color All primary colors.
Resistance to 1,1,1-Trichlorethane Conditional
Resistance to Acetic Acid (100%) Conditional
Resistance to Acetone Conditional
Resistance to Ammonium Hydroxide (50%) Recommended Conditional
Resistance to Benzene Conditional
Resistance to Brine-Saturated H2O Recommended
Resistance to Brine-Saturated H<sub>2</sub>O (310g/l)
Resistance to Chlorinated H2O Recommended
Resistance to Clorox® (10%) H2O Recommended
Resistance to Diesel Fuel Recommended Conditional
Resistance to Gasoline Recommended Conditional
Resistance to Gasoline/ 5% Methanol Recommended Conditional
Resistance to Gasoline/5% MTBE Recommended Conditional
Resistance to H2O Recommended
Resistance to H2O (14 days at 82°C) Recommended Conditional
Resistance to Hydraulic Fluid (oil) Recommended Conditional
Resistance to Hydrochloric Acid (20%) Recommended
Resistance to Hydrofluoric Acid(10%) Not Recommended
Resistance to Isopropyl Alcohol Recommended
Resistance to Lactic Acid Recommended Conditional
Resistance to MEK Recommended Conditional
Resistance to Methanol Recommended
Resistance to Methylene chloride Conditional
Resistance to Mineral Spirits Recommended Conditional
Resistance to Motor Oil Recommended
Resistance to MTEB Conditional
Resistance to Muriatic Acid (10%) Recommended
Resistance to NaCl/H2O (10%) Recommended
Resistance to Nitric Acid (20%) Not Recommended
Resistance to Phosphoric Acid (10%) Recommended
Resistance to Phosphoric Acid (50%) Not Recommended
Resistance to Potassium Hydroxide (10%) Recommended
Resistance to Potassium Hydroxide (20%) Recommended, Discoloration
Resistance to Propylene Carbonate Recommended Conditional
Resistance to Skydrol® Conditional
Resistance to Sodium Bicarbonate Recommended
Resistance to Sodium Hydroxide (25%) Recommended
Resistance to Sodium Hydroxide (50%) Recommended, Discoloration
Resistance to Sodium Hypochlorite (10%) Recommended
Resistance to Stearic Acid Recommended
Resistance to Sugar/H2O Recommended
Resistance to Sulfuric Acid (>50%) Recommended Conditional
Resistance to Sulfuric Acid (10%) Recommended
Resistance to Toluene Recommended
Resistance to Trisodium Phosphate Recommended
Resistance to Vinegar/ H2O (5%) Recommended
Resistance to Xylene Recommended Conditional