Polymer Property : Adhesive Bond Strength = 13.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 3.45 - 13.8 MPa
500 - 2000 psi
Varies with substrates
Loctite® Durabond® U-10FL Urethane Adhesive
Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap..