Mechanical Properties Metric English Comments
Adhesive Bond Strength 3.45 MPa
500 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Resinlab® SEC1244 Silver Filled Epoxy Adhesive
Resinlab™ SEC1244 is a silver filled, two component, elevated temperature curing epoxy adhesive. It provides excellent electrical conductivity useful in many electronic applications. It is a smooth..
Adhesive Bond Strength 3.45 MPa
500 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 813J01 Silicone Encapsulant
TRA-BOND 813J01 is a silicone adhesive system formulated to provide excellent thermal conductivity. This unique product bonds well to difficult substrates. Typical applications include encapsulation..
Adhesive Bond Strength 3.45 - 13.8 MPa
500 - 2000 psi
Varies with substrates
Loctite® Durabond® U-10FL Urethane Adhesive
Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap..