Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 3.45 - 13.8 MPa | 500 - 2000 psi | Varies with substrates |
Loctite® Durabond® U-10FL Urethane Adhesive Urethane AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 ap.. |