Mechanical Properties Metric English Comments
Adhesive Bond Strength 12.0 - 14.0 MPa
1740 - 2030 psi
Phenolic, Shear; ISO 4587
Permabond 101 Cyanoacrylate, Wicking Viscosity
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya..
Adhesive Bond Strength 12.0 - 14.0 MPa
1740 - 2030 psi
Phenolic, Shear; ISO 4587
Permabond 105 Cyanoacrylate, for difficult rubbers
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives..
Adhesive Bond Strength 12.0 - 14.0 MPa
1740 - 2030 psi
Mild steel, Shear
Permabond ET500 Epoxy Resin
PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera..
Adhesive Bond Strength 12.0 - 18.0 MPa
1740 - 2610 psi
Zinc, Shear
Permabond TA439 Toughened Acrylic Adhesive
Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f..
Adhesive Bond Strength 12.0 - 18.0 MPa
1740 - 2610 psi
Zinc Plated after 24 hours, Shear
Permabond TA459 Toughened Acrylic Adhesive
Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens..
Adhesive Bond Strength 12.0 - 18.0 MPa
1740 - 2610 psi
Zinc Plated after 24 hours, Shear
Permabond TA4590 Toughened Acrylic Adhesive
Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen..
Adhesive Bond Strength 12.0 - 14.0 MPa
1740 - 2030 psi
Phenolic, Shear
Permabond 102 Cyanoacrylate, General purpose
PERMABOND® 102 is a low viscosity general purpose cyanoacrylate adhesive suitable for bonding close-fitting components. It is fast setting and suitable for use on plastics, rubber and metals. Cyano..
Adhesive Bond Strength 12.0 MPa
1740 psi
Lap Shear Cohesive Strength; ASTM D1002
ITW Plexus Plexusâ„¢ 3940 Methacrylate Adhesive
An adhesive with versatile substrate and application capabilities for a wide range of industrial product assembly applications.Fast tacking, low pressure sprayable adhesive with long bonding range, ..
Adhesive Bond Strength 12.0 MPa
1740 psi
steel collar and pin shear; ISO 10123
Permabond A1042 Anaerobic Threadlocker
Permabond® A1042 is a rapid curing adhesive designed to lock and seal metal parts that subsequently may need to be dismantled for maintenance. The high vibration resistance makes Permabond A1042 pa..
Adhesive Bond Strength 12.0 MPa
1740 psi
Tensile shear per ASTM D1002 on etched Al panel
Von Roll Isola IMI E-Solder® 3083 Electrically Conductive Adhesive
Data provided by Von Roll Isola USA.E-SOLDER® epoxy based resin systems can be used at room temperature on heat sensitive materials, can bond dissimilar materials, and do not have flux or residue t..
Adhesive Bond Strength 12.0 MPa
1740 psi
steel collar and pin shear; ISO 10123
Permabond A113 Anaerobic Threadlocker
Designed for the locking and sealing of metal parts, Permabond® A113 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used ..
Adhesive Bond Strength 12.0 MPa
1740 psi
steel collar and pin shear; ISO 10123
Permabond A130 Anaerobic Threadlocker
Designed for the locking and sealing of metal parts, Permabond® A130 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used t..
Adhesive Bond Strength 12.0 MPa
1740 psi
steel collar and pin shear; ISO 10123
Permabond A136 Anaerobic Gasketmaker
Permabond® A136 is an anaerobic material designed for making 'formed in situ' gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets thereby offering potent..