Mechanical Properties Metric English Comments
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ASTM D1002
Permabond ES550 Epoxy Resin
PERMABOND ES550 is a single-part epoxy paste which is slump-resistant (does not flow) during cure. The adhesive is toughened for maximum impact resistance, along with excellent peel and shear streng..
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Aluminum, Shear; ISO 4587
Permabond ES562 Epoxy Resin
PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t..
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ISO 4587
Permabond ES562 Epoxy Resin
PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t..
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ASTM D1002
Permabond ES578 Epoxy Resin
PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bon..
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ASTM D1002
Permabond ES569 Epoxy Resin
PERMABOND® ES569 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces as well as composite materials. The high bond strength of this adhesive allows it to replace me..