Polymer Property : Adhesive Bond Strength = 6100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 6.89 - 42.1 MPa
1000 - 6100 psi
Average value: 19.1 MPa Grade Count:7
Overview of materials for Epoxy, Cast, Metal Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a..