Mechanical Properties Metric English Comments
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Adhesive Bond Strength 9.65 - 16.5 MPa
1400 - 2390 psi
Steel, Shear
Permabond QFS16 Cyanoacrylate Activator
The PERMABOND QFS 16 accelerates the cure of cyanoacrylate adhesives to provide a shorter set time. It can be used in a variety of applications but is especially useful when bonding porous or poorly..
Adhesive Bond Strength 9.65 - 36.5 MPa
1400 - 5300 psi
Average value: 25.7 MPa Grade Count:8
Overview of materials for Epoxy Adhesive, Flexible
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro..
Adhesive Bond Strength 9.65 MPa

@Thickness 12.7 mm
1400 psi

@Thickness 0.500 in
ASTM D229
Haysite H900 Polyester, Glass Reinforced
H900 is recognized throughout the world as a reliable, consistent GPO-3 material. Standard size sheets are available in thicknesses ranging from .094" to 2.00". H900 also exhibits excellent smoke,..
Adhesive Bond Strength 9.65 MPa
1400 psi
Phenolic-Phenolic; Substrate Failure; Tensile Lap Shear
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate
Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver..
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Bond 2122 Metal Repair Aluminum Epoxy Adhesive
TRA-BOND 2122 is a versatile aluminum metal filled epoxy formulation developed for modern industrial casting, bonding and repair applications where a strong aluminum-like adhesive is required. This ..
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap shear, alum to alum, 7 days in water
Tra-Con Tra-Bond 5126 Medium Viscosity Aerospace-Grade Epoxy Adhesive
TRA-BOND 5126 AEROSPACE-GRADE EPOXY ADHESIVE is a two-part, clear (amber), medium viscosity, aerospace-grade epoxy adhesive system recommended for bonding a wide variety of materials for structural ..
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap shear, alum to alum, 15 min @ 120°C
Tra-Con Tra-Bond 546S04 Thixotropic UV/Blue Light Cure Adhesive
TRA-BOND 546S04 is a thixotropic UV/blue light curable adhesive with a secondary heat cure. TRA-BOND 546S04 is ideal for general optics bonding, mounting of lenses, and glob top applications. The ..
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap shear, alum to alum, 1 hr @ 150°C
Tra-Con Tra-Duct 8205 One-Part Electrically Conductive Silver-Filled Epoxy
TRA-DUCT 8205 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of excellent mechanical and electrical..
Adhesive Bond Strength 9.65 MPa
1400 psi
Trelleborg Emerson & Cuming Eccobond® 927-10 E Needle Bonding Epoxy Adhesive
Emerson & Cuming 927-10 E Eccobond® Needle Bonding Epoxy AdhesiveOne component, fast curing, epoxy adhesive for needle bonding with polypropylene hubs. Also recommended for bonding sealing or insul..
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap Shear Strength
Epoxyset Epoxibond EB-109M-4 Unfilled Epoxy Adhesive
A two-component, unfilled, flexible epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-109M-4 puts low stress on fragile parts a..
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap Shear Strength
Epoxyset Epoxiohm EO-21M-5 Electrically Conductive Epoxy Adhesive
EO-21M-5 is an electrically conductive & thermally conductive, silver filled epoxy adhesive. This two component system is designed to be cured at room temperature or the cure can be accelerated by e..
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap Shear Strength
Epoxyset Epoxiohm EO-24 Electrically Conductive Epoxy Adhesive
EO-24 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management applica..
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap Shear Strength
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive
EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy ..
Adhesive Bond Strength 9.65 MPa

@Temperature 82.2 °C
1400 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
Armstrong A-3/A Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..
Adhesive Bond Strength 9.65 MPa

@Temperature 25.0 °C
1400 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
Armstrong C-4/D Epoxy Adhesive
A low viscosity, clear amber, unfilled adhesive, recommended for use with activators D or W. C-4 with Activator W offers maximum versatility in that differing degrees of flexibility can be achieved ..
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 872-3 Flexible Epoxy Adhesive
TRA-BOND 872-3 transparent, flexible epoxy adhesive is designed for bonding materials with mismatched coefficients of thermal expansion. The long working life of this adhesive makes it ideal for use..
Adhesive Bond Strength 9.65 MPa
1400 psi
Rogers Test Method
Rogers Corporation 3001 Thermoplastic Chloro-Fluorocopolymer Bonding Film