Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00469 GPa | 0.680 ksi | ASTM D638 |
Multibase Multi-Flex® TPE A 5904 LC BLK Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and fe.. |
|||
300% Modulus | 0.00469 GPa @Time 7200 sec |
0.680 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-80-1000 TPE Product Description: StarXTRUDE XTR-80-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |