Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 0.680 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00469 GPa
0.680 ksi
ASTM D638
Multibase Multi-Flex® TPE A 5904 LC BLK
Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and fe..
300% Modulus 0.00469 GPa

@Time 7200 sec
0.680 ksi

@Time 2.00 hour
Die C; ASTM D412
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-80-1000 TPE
Product Description: StarXTRUDE XTR-80-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P..
Copyright © lookpolymers.com All Rights Reserved