Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 0.0290 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0290 GPa
4.21 ksi
ISO 37
Huntsman AVALON® 98 AB Thermoplastic Polyurethane
Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma..
300% Modulus 0.0290 GPa
4.21 ksi
ASTM D412
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos..
300% Modulus 0.0290 GPa
4.21 ksi
ASTM D412
Wanhua Chemical Wanthane® WHT-1195 Polyester Based TPU
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
300% Modulus 0.0290 GPa
4.21 ksi
ISO 37
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in..
300% Modulus 0.0290 GPa
4.21 ksi
ASTM D412
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
300% Modulus 0.0290 GPa
4.21 ksi
ASTM D412
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: ..