Polymer Property : 300% Modulus = 0.149 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00103 GPa
0.149 ksi
Transverse Direction; Injection molded sample tested at 10 in/min with Die D; ASTM D412
Kraton® D2104 DI-N (SBS) Compound
Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D..
300% Modulus 0.00103 GPa
0.149 ksi
Typical properties based on film cast from toluene solution.; ASTM D412
Kraton® D4150 K (SBS) Linear Block Copolymer
Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton..
300% Modulus 0.00103 GPa
0.149 ksi
Measured on films cast from a solution in toluene; ASTM D412
Kraton® D4433 P (O/E SIS) Linear Triblock Copolymer
Description: Kraton D4433 P is an oiled, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified:..
300% Modulus 0.00103 GPa
0.149 ksi
Typical properties based on film cast from toluene solution.; ASTM D412
Kraton® D4433 P (SIS) Linear Block Copolymer
Description: Kraton D4433 P is an oiled, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified:..