Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 47.5 J @Temperature 22.2 °C |
35.0 ft-lb @Temperature 72.0 °F |
0.125 in.; ARM test |
Polimeros Mexicanos Rotolene® Black Plus Ultra Polyethylene Linear copolymer Medium Density Polyethylene which is fully UV8 stabilized. Available as black powder.Applications: Polyethylene compound specially formulated for rotational molding applications req.. |
|||
Impact Test | 47.5 J @Temperature 22.2 °C |
35.0 ft-lb @Temperature 72.0 °F |
ARM STD test |
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer, available as black powder.Recommended for rotomolding. Used for manufacture of septic tanks and garbage bins. Recommended for use in combination with ROTOFOAM B.. |
|||
Impact Test | 47.5 J @Temperature -40.0 °C |
35.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy: 0.100-in.; 0.5-in. dart; 1.6-in. clamp; 7.6 mph; ASTM-D3763 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Impact Test | 47.5 J | 35.0 ft-lb | Torque Strength; curing at 1000°F |
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Impact Test | 47.5 J @Temperature -29.0 °C |
35.0 ft-lb @Temperature -20.2 °F |
ASTM D3763 |
Braskem TI6120Q4 High Impact Copolymer Polypropylene Description: Extra High Izod Impact, Superior Low Temperature Drop Impact, Good Paint AdhesionApplications: Suggested Uses Include Compounding, Automotive, Injection MoldingThis resin meets the requ.. |
|||
Impact Test | 47.5 J @Temperature -29.0 °C |
35.0 ft-lb @Temperature -20.2 °F |
ASTM D3763 |
Braskem TI6200Q4 High impact Copolymer Polypropylene Description: Extra high izod impact, superior low temperature drop impact, good paint adhesion. Applications: Suggested uses include toys, video cassettes, compounding. Process: Compounding. This r.. |
|||
Impact Test | 47.5 J @Temperature -29.0 °C |
35.0 ft-lb @Temperature -20.2 °F |
ASTM D3763 |
Braskem TI6120AN High Impact Copolymer Polypropylene Description: Excellent balance of toughness and stiffness, unique dimensional stability and excellent flow properties.Applications: Suggested uses include compounding, injection molding, automotive .. |