Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer Polimeros Mexicanos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MDPE Copolymer with UV8 stabilizer, available as black powder.Recommended for rotomolding. Used for manufacture of septic tanks and garbage bins. Recommended for use in combination with ROTOFOAM BLACK for multi-layer containers. Contains mold release agents. Meets all FDA 21 CFR 177.1520 and CONEG (as a compound), covering safe use in articles intended for direct food contact.Information provided by Polimeros Mexicanos
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 750 hour
>= 750 hour
ASTM D1693
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 11.7 MPa
1700 psi
2 in/min; ASTM D638
Tensile Strength, Yield 21.4 MPa
3100 psi
2 in/min; ASTM D638
Elongation at Break >= 400 %
>= 400 %
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 0.758 GPa
110 ksi
1% Secant; ASTM D790
Impact Test 47.5 J

@Temperature 22.2 °C
35.0 ft-lb

@Temperature 72.0 °F
ARM STD test
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
ASTM D648
Descriptive Properties Value Comments
Process Rotational Molding
Region Europe/Turkey
Bamberger Polymers Distribution