Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 47.5 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 47.5 J

@Temperature 22.2 °C
35.0 ft-lb

@Temperature 72.0 °F
0.125 in.; ARM test
Polimeros Mexicanos Rotolene® Black Plus Ultra Polyethylene
Linear copolymer Medium Density Polyethylene which is fully UV8 stabilized. Available as black powder.Applications: Polyethylene compound specially formulated for rotational molding applications req..
Impact Test 47.5 J

@Temperature 22.2 °C
35.0 ft-lb

@Temperature 72.0 °F
ARM STD test
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene
MDPE Copolymer with UV8 stabilizer, available as black powder.Recommended for rotomolding. Used for manufacture of septic tanks and garbage bins. Recommended for use in combination with ROTOFOAM B..
Impact Test 47.5 J

@Temperature -40.0 °C
35.0 ft-lb

@Temperature -40.0 °F
Instrumented Impact, Total Energy: 0.100-in.; 0.5-in. dart; 1.6-in. clamp; 7.6 mph; ASTM-D3763
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Impact Test 47.5 J
35.0 ft-lb
Torque Strength; curing at 1000°F
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and..
Impact Test 47.5 J

@Temperature -29.0 °C
35.0 ft-lb

@Temperature -20.2 °F
ASTM D3763
Braskem TI6120Q4 High Impact Copolymer Polypropylene
Description: Extra High Izod Impact, Superior Low Temperature Drop Impact, Good Paint AdhesionApplications: Suggested Uses Include Compounding, Automotive, Injection MoldingThis resin meets the requ..
Impact Test 47.5 J

@Temperature -29.0 °C
35.0 ft-lb

@Temperature -20.2 °F
ASTM D3763
Braskem TI6200Q4 High impact Copolymer Polypropylene
Description: Extra high izod impact, superior low temperature drop impact, good paint adhesion. Applications: Suggested uses include toys, video cassettes, compounding. Process: Compounding. This r..
Impact Test 47.5 J

@Temperature -29.0 °C
35.0 ft-lb

@Temperature -20.2 °F
ASTM D3763
Braskem TI6120AN High Impact Copolymer Polypropylene
Description: Excellent balance of toughness and stiffness, unique dimensional stability and excellent flow properties.Applications: Suggested uses include compounding, injection molding, automotive ..