Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.220 J/cm @Temperature 23.0 °C |
0.412 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® INP562 ABS SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature -30.0 °C |
0.412 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® INP563 ABS SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature -30.0 °C |
0.412 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® INP564 ABS SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature -40.0 °C |
0.412 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature -20.0 °C |
0.412 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
LATI LARIL 13-V1KC Mineral Filled Polyphenylene Oxide (PPOm) (UL94V-1)
(Unverified Data**) Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most .. |
|||
Izod Impact, Notched | 0.220 J/cm @Temperature -20.0 °C |
0.412 ft-lb/in @Temperature -4.00 °F |
ASTM-D256 |
Braskem CP 202XP HECO Polypropylene Heterophasic Copolymer CP 202XP is a high melt flow rate heterophasic copolymer designed to achieve parts with high stiffness and impact strength resistance, low warpage, and excellent surface appearance. Its applications.. |