Polymer Property : Izod Impact, Notched = 0.670 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.670 J/cm

@Temperature 23.0 °C
1.26 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy EXGY30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.670 J/cm

@Temperature 23.0 °C
1.26 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy FXTW30PE ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.670 J/cm

@Temperature 23.0 °C
1.26 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Geloy FXTW30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.670 J/cm

@Temperature 23.0 °C
1.26 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Eastar EN076 Copolyester
Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o..
Izod Impact, Notched 0.670 J/cm

@Temperature -20.0 °C
1.26 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
Braskem PCD 0810 HECO Polypropylene Heterophasic Copolymer
PCD 0810 is a high melt flow rate heterophasic copolymer developed for injection molding applications. The product combines high impact strength and good processability with a fair stiffness level. ..
Izod Impact, Notched 0.670 J/cm

@Temperature -20.0 °C
1.26 ft-lb/in

@Temperature -4.00 °F
ASTM D256
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..