Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.17 J/cm @Temperature -40.0 °C |
2.19 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
DuPont Performance Polymers Crastin® ST820 BK503 PBT
(Unverified Data**) Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.17 J/cm @Temperature 23.0 °C |
2.20 ft-lb/in @Temperature 73.4 °F |
1/8'' notched bar; ASTM D256 |
Ineos L12N-00 Polypropylene Impact Copolymer This is a medium melt flow rate, nucleated impact copolymer polypropylene for injection molding and compounding applications. This material meets the requirements of the U.S. Food and Drug Administ.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.20 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF34 IM HS 34% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 34% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
2.20 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearanc.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
2.20 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF25 FR-N IM3 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedAppearance: RedInformation provi.. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
2.19 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Diamond Polymers Centrex® 833 Sheet Extrusion Grade Centrex 833 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it .. |
|||
Izod Impact, Notched | 1.17 J/cm @Thickness 6.35 mm |
2.20 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 2512 Rigid PVC, Extrusion Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |