Polymer Property : Izod Impact, Notched = 2.40 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.40 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.50 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Ineos ABS Lustran® LK197 ABS, Extrusion Grade
Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e..
Izod Impact, Notched 2.40 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
4.50 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8003
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp..
Izod Impact, Notched 2.40 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
4.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8007
Availability: North AmericaForms: PelletsFeatures: General Purpose and High FlowInformation provided by TP Composites, Inc.
Izod Impact, Notched 2.40 J/cm

@Thickness 3.17 mm
4.50 ft-lb/in

@Thickness 0.125 in
ASTM Test
Styrolution Terluran® GP-35 ABS
Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an..
Izod Impact, Notched 2.40 J/cm

@Temperature 22.8 °C
4.50 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade
Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W..
Izod Impact, Notched 2.40 J/cm

@Temperature -40.0 °C
4.50 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Teknor Apex Chemlon® 109 Nylon 66, Impact Grade
Notes: High-Impact; Exceptional impact strength, especially at low temperatures; FMVSS Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
Izod Impact, Notched 2.40 J/cm

@Thickness 6.35 mm
4.50 ft-lb/in

@Thickness 0.250 in
TPI Porene® ABS-GA803 High Gloss, UV Resistant ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 2.40 J/cm

@Temperature 23.0 °C
4.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 550E3V45510 Cellulose Acetate Butyrate, Water Clear, Trsp
Applications:AppliancesConsumer-Personal careProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gl..
Izod Impact, Notched 2.40 J/cm

@Temperature 23.0 °C
4.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Eastman Tenite 550E3V45510 Butyrate Water Clear, Trsp  (discontinued **)
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..