Polymer Property : Izod Impact, Notched = 2.45 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.96 - 2.45 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
3.67 - 4.59 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Samyang Triel® 5722EM Thermoplastics Polyetherester Elastomer, Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5722EM is an extrusion grade.Information provided by Samyang.