Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 3.74 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.74 J/cm

@Temperature -40.0 °C
7.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
Izod Impact, Notched 3.74 J/cm

@Temperature 22.8 °C
7.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte..
Izod Impact, Notched 3.74 J/cm

@Temperature 22.8 °C
7.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Izod Impact, Notched 3.74 J/cm

@Temperature 22.8 °C
7.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Izod Impact, Notched 3.74 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
7.01 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Ineos ABS Lustran® 750 ABS, Molding Grade
Lustran® 750 resin is a black, virgin injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is designed for molded drain, waste, and vent (DWV) fittings. Lustran® 750 (901802 bl..
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
7.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/66 IM 6040 MB
Availability: North AmericaForms: PelletsAdditive: Nucleating Agent, Heat Stabilizer, Lubricant and Impact ModifierFeatures: Copolymer, Nucleated, Heat Stabilized, Lubricant and Impact ModifiedInfor..
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
7.00 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 7000
Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc.
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
7.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 7000
Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc.
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
7.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8003
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp..
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
7.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8004 FR
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
7.00 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® PC/ABS 2110 BK
Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 3.74 J/cm

@Thickness 6.35 mm,
Temperature -30.0 °C
7.00 ft-lb/in

@Thickness 0.250 in,
Temperature -22.0 °F
ASTM D256
PlastxWorld CEVIAN® S1100 High Impact PC/ABS alloy
These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
7.01 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Diamond Polymers DIAMALOY PC 1812 Impact Modified Polycarbonate
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm
7.00 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall ProTherm® 4345 Rigid PVC, Extrusion
Georgia Gulf ProTherm® 4345 is a CPVC powder blend designed for extrusion applications requiring high heat deflection temperatures. Processing and stability along with overall physical properties ..