Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LUPOY SC1004AU PC, High Impact

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Impact Modified
Manufacturer LG Chemical
Trade Name LUPOY
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUPOY SC1004AU PC, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Maximum Moisture Content 0.020
0.020
Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 22 g/10 min

@Load 1.20 kg,
Temperature 300 °C
22 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 54.9 MPa

@Thickness 3.20 mm
7970 psi

@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 130 %

@Thickness 3.20 mm
130 %

@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 89.2 MPa

@Thickness 3.20 mm
12900 psi

@Thickness 0.126 in
10mm/min; ASTM D790
Flexural Modulus 2.11 GPa

@Thickness 3.20 mm
306 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
Izod Impact, Notched >= 2.94 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
>= 5.51 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
>= 5.88 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 11.0 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C

@Thickness 6.40 mm
257 °F

@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 80.0 °C

@Thickness >=0.700 mm
176 °F

@Thickness >=0.0276 in
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=0.700 mm
176 °F

@Thickness >=0.0276 in
UL RTI, Mechanical without Impact 80.0 °C

@Thickness >=0.700 mm
176 °F

@Thickness >=0.0276 in
Flammability, UL94 HB

@Thickness >=0.700 mm
HB

@Thickness >=0.0276 in
Processing Properties Metric English Comments
Rear Barrel Temperature 275 - 290 °C
527 - 554 °F
Injection Molding
Middle Barrel Temperature 280 - 295 °C
536 - 563 °F
Injection Molding
Front Barrel Temperature 290 - 300 °C
554 - 572 °F
Injection Molding
Nozzle Temperature 285 - 300 °C
545 - 572 °F
Injection Molding
Melt Temperature 285 - 300 °C
545 - 572 °F
Injection Molding
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Injection Molding
Drying Temperature 100 - 110 °C
212 - 230 °F
Injection Molding
Dry Time 3.00 - 5.00 hour
3.00 - 5.00 hour
Injection Molding
Back Pressure 0.981 - 3.92 MPa
142 - 569 psi
Injection Molding
Screw Speed 40 - 70 rpm
40 - 70 rpm
Injection Molding
Users viewing this material also viewed the following: