Polymer Property : Izod Impact, Notched = 6.46 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.45 J/cm

@Temperature 23.0 °C
6.46 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL4019 PC (Europe-Africa-Middle East)
Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im..
Izod Impact, Notched 3.45 J/cm

@Temperature -20.0 °C
6.46 ft-lb/in

@Temperature -4.00 °F
ASTM D 256
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East)
XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.