Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 233 GPa @Temperature 25.6 °C |
33800 ksi @Temperature 78.1 °F |
Annealed |
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |