Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 233 GPa

@Temperature 25.6 °C
33800 ksi

@Temperature 78.1 °F
Annealed
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers..