Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 87.56 MPa @Strain 1.35 %, Temperature 0.000 °C |
12700 psi @Strain 1.35 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Stress | 87.3 MPa @Strain 4.00 %, Temperature -40.0 °C |
12700 psi @Strain 4.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |
|||
Tensile Stress | 87.56 MPa @Strain 2.16 %, Temperature 0.000 °C |
12700 psi @Strain 2.16 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) 20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf.. |
|||
Tensile Stress | 87.57 MPa @Strain 1.87 %, Temperature 40.0 °C |
12700 psi @Strain 1.87 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 87.5 MPa @Strain 4.20 %, Temperature -40.0 °C |
12700 psi @Strain 4.20 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |
|||
Tensile Stress | 87.5 MPa @Strain 0.880 %, Temperature -20.0 °C |
12700 psi @Strain 0.880 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Stress | 87.7 MPa @Strain 1.50 %, Temperature 23.0 °C |
12700 psi @Strain 1.50 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Tensile Stress | 87.6 MPa @Strain 1.82 %, Temperature 40.0 °C |
12700 psi @Strain 1.82 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR515 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 NC010 is a flame retardant 15% glass reinforced modified polyethylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm.. |