Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 92.8 MPa @Strain 13.0 %, Temperature -40.0 °C |
13500 psi @Strain 13.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Stress | 93.2 MPa @Strain 4.40 %, Temperature -40.0 °C |
13500 psi @Strain 4.40 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Tensile Stress | 92.8 MPa @Strain 13.0 %, Temperature -40.0 °C |
13500 psi @Strain 13.0 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Stress | 93.2 MPa @Strain 4.40 %, Temperature -40.0 °C |
13500 psi @Strain 4.40 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Tensile Stress | 92.9 MPa @Strain 2.00 %, Temperature 23.0 °C |
13500 psi @Strain 2.00 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 93.07 MPa @Strain 1.19 %, Temperature 40.0 °C |
13500 psi @Strain 1.19 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |
|||
Tensile Stress | 93.0 MPa @Strain 6.00 %, Temperature -40.0 °C |
13500 psi @Strain 6.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 92.9 MPa @Strain 3.36 %, Temperature 23.0 °C |
13500 psi @Strain 3.36 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |