Mechanical Properties Metric English Comments
Tensile Stress 0.951 MPa

@Strain 300 %,
Temperature 23.0 °C
138 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE)
Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough..
Tensile Stress 0.951 MPa

@Strain 100 %
138 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3935T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress >= 0.951 MPa

@Strain 50.0 %
>= 138 psi

@Strain 50.0 %
ASTM D412 Method A
Seals Eastern 5722A Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Exce..
Tensile Stress 0.950 MPa

@Strain 0.000 %,
Temperature 120 °C
138 psi

@Strain 0.000 %,
Temperature 248 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Stress 0.950 MPa

@Strain 0.0600 %,
Temperature -20.0 °C
138 psi

@Strain 0.0600 %,
Temperature -4.00 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..