Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.30 MPa @Strain 100 % |
189 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KG 40A-3S2016 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Stress | 1.30 MPa @Strain 100 % |
189 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® N8950 TPE, Nylon Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se.. |
|||
Tensile Stress | 1.30 MPa @Strain 100 % |
189 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3850H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.30 MPa @Strain 100 % |
189 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P52-004A-3B TPE, PP Overmold or Standalone use Characteristics: Soft, flexible feelExcellent grip characteristicsGood weatherabilityGood compression setEasy processability and colorabilityAvailable FDA and medical gradesAvailable translucent gra.. |
|||
Tensile Stress | 1.30 MPa @Strain 5.00 %, Temperature 100 °C |
189 psi @Strain 5.00 %, Temperature 212 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Tensile Stress | 1.30 MPa @Strain 100 % |
189 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G45A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G45A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 1.30 MPa @Strain 100 % |
189 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G45A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G45A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |