Material Notes:
OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide polymers including PA6, PA6.6, PA11 and PA12. OnFlex™-S KG can be processed by 2K molding or overmolding, insert molding or co-extrusion. In addition to this, OnFlex™-S KG compounds are formulated to provide good processability and a good cost/performance ratio, a wide hardness range, good colourability and good mechanical properties.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
ISO 868
Tensile Strength at Break 2.60 MPa
377 psi
ISO 37
Tensile Stress 1.30 MPa

@Strain 100 %
189 psi

@Strain 100 %
ISO 37
2.20 MPa

@Strain 300 %
319 psi

@Strain 300 %
ISO 37
Elongation at Break 330 %
330 %
ISO 37
Tear Strength 16.0 kN/m
91.3 pli
ISO 34-1
Compression Set 31 %

@Temperature 23.0 °C,
Time 259000 sec
31 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
62 %

@Temperature 70.0 °C,
Time 79200 sec
62 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
80 %

@Temperature 100 °C,
Time 79200 sec
80 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Processing Properties Metric English Comments
Melt Temperature 200 - 260 °C
392 - 500 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Drying Temperature 100 °C
212 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Features General Purpose
Good Adhesion
Forms Pellets
Generic Material TPE
Generic Material Type Styrenic Thermoplastic Elastomer (TES)
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Moderate
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Coextrusion
Multi Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Automotive Applications
Consumer Applications
Industrial Applications
Overmolding
Power/Other Tools